ANTI-WRINKLE BASE

Manufacturing Process Phase A: Disperse the thickeners in glycerol and Cosphaderm® Propanediol natural. Phase B: Add demin. water and stir until everything is dissolved. Phase C: Add phase C to A/B. Adjust the pH to 5.5 +_ 0.05. Specification Appearance: Translucent, viscous gel pH: 5.5 +_ 0.05 Stability: No separation after centrifugation (4000 rpm, 30 min), stable for 3 months at room temperaturehas not

ANTI-POLLUTION SERUM

MANUFACTURING PROCESS Phase A: Combine all ingredients of phase A and stir until everything is completely dissolved. Phase B: Combine all ingredients of phase B. Heat both phases separately to 70-75 °C and add phase B to A while stirring. Then homogenise the formulation. Phase C: Dissolve Cosphaderm® Magnolia Extract 98 in Cosphaderm® Dicapo natural. Add phase C and phase D to phase A+B after coolinghas not

JELLY SOAP

Manufacturing Process Phase A: Prepare phase A and stir until dispersed. Phase B: Slowly add the water to phase A under stirring and stir until complete dissolution. If wanted, add heat-proof colour. Phase C: Prepare phase C, adjust the pH to 5.5 +_ 0.05 and set aside. Heat phase A+B to its boiling point and keep this temperature for 2 - 3 min. Add phase C to the hot phase A+B. Continue stirring until ehas not

SOOTHING BODY LOTION

MANUFACTURING PROCESS Phase A: Combine all ingredients of phase A and stir until everything is completely dissolved. Phase B: Add phase B to the water phase while stirring. Then heat the water phase to 70-75 °C. Phase C: Combine all ingredients of phase C and heat to 75°C. Add phase C to the water phase while stirring. Add phase D to the emulsion and homogenise. Adjust the pH to 5.5 +_ 0.05. SPECIFIhas not
Register now for the Newsletter!

DEODORANT ROLL-ON

Manufacturing Process Phase A: Combine all ingredients of phase A and stir until everything is completely dissolved. Phase B: Combine all ingredients of phase B. Heat both phases separately to 75 °C and add phase B to A while stirring very fast. Homogenise. Adjust the pH to 5.0 +_ 0.05. Specification Appearance: White viscous lotion pH: 5.0 +_ 0.05 Stability: No separation after centrifugation (400has not

CALM & CARE FLUID

MANUFACTURING PROCESS Phase A: Combine all ingredients of phase A and stir until everything is completely dissolved. Heat to 70-75 °C. Phase B: Combine all ingredients and heat to 75 °C. Add then phase B to phase A under strong stirring and homogenise. Phase C: Dissolve Cosphaderm® Panthenol natural in water and add phase C below 40 °C. Adjust the pH to 5.5 +_ 0.05. SPECIFICATION Appearance: Whitehas not

CREAMY BLUSH STICK

MANUFACTURING PROCESS Phase A: Mix all ingredients together and heat to 80-85 °C until everything is melted. Phase B: Add all ingredients of phase B to phase A at 70°C. Phase C: Premix the pigments in the oils until everything is homogeneous and add it to the hot phase A+B and fill into packaging. SPECIFICATION Appearance: Solid stick Stability: stable for 3 months at room temperature and 40 °C Mihas not

NOURISHING SHAVING OIL

MANUFACTURING PROCESS Combine all ingredients of phase A and melt until everything is homogeneous. SPECIFICATION Appearance: Cloudy, thickened oil Stability: Stable for 3 months at room temperature and 40 °C Microbiological stability: proven (Water activity value less than 0.75)has not
×